Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Definition of "pea rock" (or "pea gravel")?

Status
Not open for further replies.

Dennis59

Structural
Joined
Dec 29, 2000
Messages
56
Location
US
Does anyone have an industry-standard gradation for either of these terms?

Thanks!
 
It's usually 1/4 to 3/8 inch gravel - but this can vary.

[pacman]

Please see FAQ731-376 for great suggestions on how to make the best use of Eng-Tips Fora. See faq158-922 for recommendations regarding the question, "How Do You Evaluate Fill Settlement Beneath Structures?"
 
how about AASHTO M43 (ASTM D 448) No. 8 or 89 gravel
 
Typically No. 89 gradation (ASTM C33)
 
Dennis59

This is a city spec from Regina, Saskatchewan, Canada.

Pea Gravel*

Sieve Size Percent Passing by Weight
12.5 mm 100%
10 mm 90 - 100%
5 mm 0 - 10%
2 mm 0 - 1%

* This material shall be clean naturally rounded aggregate.

The naturally rounded/nonfractured part can be important depending on the application (ie. naturally rounded stone should be used when pea gravel is being placed against a geomembrane or drain tile to eliminate puncturing).

Hope this helps.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top