fordosrobi
Student
- Feb 24, 2022
- 1
Hi there!
I am trying to simulate a honeycomb pattern core material, and I can't figure out what means what in the datasheet and the Abaqus material card.
My questions are what do the D1111 D1122... cells mean? I have access to the following properties of the material:
Compressive Bare Strength, Compressive Stabilized Strength, Compressive Stabilized Modulus, Plate shear L direction strength and modulus, Plate shear W direction strength and modulus.
I have also attatched the datasheet of the material. It is the "HRH-10 – 3/16 – 3.0" the one I need to simulate.
Thank you for the help in advance!
Best regards, Róbert
I am trying to simulate a honeycomb pattern core material, and I can't figure out what means what in the datasheet and the Abaqus material card.
My questions are what do the D1111 D1122... cells mean? I have access to the following properties of the material:
Compressive Bare Strength, Compressive Stabilized Strength, Compressive Stabilized Modulus, Plate shear L direction strength and modulus, Plate shear W direction strength and modulus.
I have also attatched the datasheet of the material. It is the "HRH-10 – 3/16 – 3.0" the one I need to simulate.
Thank you for the help in advance!
Best regards, Róbert