Hi Guys,
I just want to know what is the differences between ASTM A105 and ASTM A234.
I have choose ASTM A234 for my utility water line, but supplier supply to me ASTM A105, so is that ok?

thank you.

Best Regards,

Antonio.
 
Replies continue below

Recommended for you

ASTM A105 is forging and ASTM A234 is wrought with A105 typically used for flanges and threaded/socket fittings and A234 used for butt welding fittings.