Feb 23, 2009 #1 TimBow123 Mechanical Joined Oct 17, 2007 Messages 12 Location US I was wondering if anyone can recommend a good guide / handbook for design of deep drawn parts, in particular with Stainless Steel. Any help would be appreciated
I was wondering if anyone can recommend a good guide / handbook for design of deep drawn parts, in particular with Stainless Steel. Any help would be appreciated
Feb 26, 2009 #2 JMarv Mechanical Joined Jul 26, 2007 Messages 188 Location US Here's a two part article from Metalforming magazine. Part 1 Part 2 Joe SW Office 2008 SP5.0 P4 3.0Ghz 3GB ATI FireGL X1 Upvote 0 Downvote
Here's a two part article from Metalforming magazine. Part 1 Part 2 Joe SW Office 2008 SP5.0 P4 3.0Ghz 3GB ATI FireGL X1
Feb 26, 2009 #3 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US STAMPING Journal is another excellent online resource for this type of information. Look through the archive of their technical articles: http://www.thefabricator.com/ToolandDie/ToolandDie_ArticleList.cfm Upvote 0 Downvote
STAMPING Journal is another excellent online resource for this type of information. Look through the archive of their technical articles: http://www.thefabricator.com/ToolandDie/ToolandDie_ArticleList.cfm
Feb 26, 2009 #4 dvd Mechanical Joined Nov 12, 2001 Messages 2,043 Location US the Metals Handbook 8th edition, volume 4 "Forming" is pretty good. I recall preferring it over 9th edition. I used those books twenty years ago. I haven't seen the latest version but you could check it out. Go to http://asmcommunity.asminternational.org/portal/site/www/ type "forming" in the search area and see books and articles available. Upvote 0 Downvote
the Metals Handbook 8th edition, volume 4 "Forming" is pretty good. I recall preferring it over 9th edition. I used those books twenty years ago. I haven't seen the latest version but you could check it out. Go to http://asmcommunity.asminternational.org/portal/site/www/ type "forming" in the search area and see books and articles available.