Hello I have to make such deep drawing part:
Can anybody help me how to fit die radius and clearance between punch and die.
There is the rule that die radius it is (4-8)t (where t is plate thickness). So it should be between 1,6 - 3,2 mm, but a cup radius it is 1mm.
And I calculated that punch diameter should be d=4,92 mm.
And the inside diameter of die has to be the same as outside diameter of cup? So 6mm?
Can anybody check it?

Can anybody help me how to fit die radius and clearance between punch and die.
There is the rule that die radius it is (4-8)t (where t is plate thickness). So it should be between 1,6 - 3,2 mm, but a cup radius it is 1mm.
And I calculated that punch diameter should be d=4,92 mm.
And the inside diameter of die has to be the same as outside diameter of cup? So 6mm?
Can anybody check it?