ripaldee
Mechanical
- Jun 16, 2011
- 22
During installation of a SS control valve it was found that the hex nut is in contact with the body of the control valve. This happened because an insulating gasket (i.e. dissimilar material and raw water service) is used in the flanged connection; thereby, it increased the bolt length causing the hex nut to clash with valve body. Now, is it possible to decrease the height of the hex nut (i.e. by grinding or machining, for example)? Does the industry code/standards allow this practice?