The summerized specs read:
for normal weight concrete air content =
•no entrained air for concrete placed in foundation
•5% +- 1.5% entrained air UNO
•3% +- 1.0% entrained air for mixes with compressive strength greater than or equal to 5000 psi
•4% +- 1.0% entrained air for mixes with compressive strength less than or equal to 5000 psi placed in aggressive
(Aggressive environment = Exterior)
So for slab-on-grade with interior exposure and placed with 4000 psi concrete the air requirement is ______?
By the specs given it's either 5+-1% OR the member is considered part of the foundation and thus no A/E required.
for normal weight concrete air content =
•no entrained air for concrete placed in foundation
•5% +- 1.5% entrained air UNO
•3% +- 1.0% entrained air for mixes with compressive strength greater than or equal to 5000 psi
•4% +- 1.0% entrained air for mixes with compressive strength less than or equal to 5000 psi placed in aggressive
(Aggressive environment = Exterior)
So for slab-on-grade with interior exposure and placed with 4000 psi concrete the air requirement is ______?
By the specs given it's either 5+-1% OR the member is considered part of the foundation and thus no A/E required.