Dear Fellows, I need to weld a flange of SA-350 LF2 Cl1 neck thickness 12.7 with shell of SA-516 Gr.70 of same thickness (Joint Cat. B weld). Is it mandatory to PWHT the weld with reference to ASME VIII Div.1-2019?
 
No. But it could be a client requirement that supersedes Div I.

DHURJATI SEN


 
1) Categoty is C (not B)
2) Is lethal or low temperature service?

Regards
 