Dear Engineers,
Could you help me to identify related literature on melting and casting of nickel and nickel base alloy(monel)for manufacturing of castings. This is to have a project development on these alloys.

s.saravanan
 
ASM HANDBOOK Volume 15 Casting is an excellent reference on castings in general, and has a section on nickel-based alloys. You can obtain this book from ASM International at
You can also perform a search of the ASM Archive for nickel-related references. The link is
You may be able to obtain useful information from various nickel-alloy producers such as Special Metals ( Allegheny Ludlum ( Carpenter ( or Krupp VDM (
 