Dear All,
We produce A234, A420 and A403 material steel elbows. We have a lab in the factory and we perform the chemical and mechanical tests here. For the small sizes A420 material elbows (OD less than 3"), can you please help me about how we prepare tensile test specimen in accordance with ASTM A420? Due to small size limitation, I can not cut the specimens in the correct dimensions needed. Thank you in advance.
We produce A234, A420 and A403 material steel elbows. We have a lab in the factory and we perform the chemical and mechanical tests here. For the small sizes A420 material elbows (OD less than 3"), can you please help me about how we prepare tensile test specimen in accordance with ASTM A420? Due to small size limitation, I can not cut the specimens in the correct dimensions needed. Thank you in advance.