Dear All
I need your help with this matter.
For material A335 P36 what is the P number for this alloy steel group?
Can someone advise me?
Thank you in advance.

 
Replies continue below

Recommended for you

Nominal composition of P36 is in between P1 & P2 although heat treatment is quite different. You can choose 3 as the P number for P36, same as that of P1 & P2.