Hello,
I'm looking into a cooling problem. Some of the potential solutions require gun drilling (~1.4m deep) through stainless steel. In order to create the cooling channel network the deep drilling will create some dead legs in the system. Is there a standard way of blocking off dead legs? I've got a few ideas about plugs etc. but don't want to reinvent the wheel if there is a standard solution out there. The environment will be hostile so polymers are probably not acceptable.
Many thanks
George
 
When a shell and tube heat exchanger tube develops a leak, it is often put back in service at reduced capacity by plugging both ends of the leaky tube. The plugs usually comprise a flanged cylinder with a tapered bore, and a tapered pin that is driven into the cylinder bore with a big hammer, expanding the cylinder against the tubewall inside the tubesheet.

The plugs are available commercially.



Mike Halloran
Pembroke Pines, FL, USA
 
There are better plugs available that are called pop-a-plug. They use a nut to draw the taper together.
More reliable than drive plugs.
You really need to gun drill? There is no room to remove heat from a surface? Those are going to be very expensive holes.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Thanks for the replies, I'll look into pop-a-plug. Gun drilling looks to be the only viable option at the moment. Thanks
George
 
If the diameter of the hole is around 1/2" or less, you can use a Lee plug. Lee plugs are very reliable, easy to install, and can handle high pressures.
 