LarryDavid
Mechanical
Hi there,
What are peoples thoughts on de-rating the tensile strength of bolts which have been galvanised?
I am designing multiple flanges which will be assembled using AS4291 / AS1110 Grade 8.8 bolts which will be galvanized. I realise that hydrogen embrittlement generally occurs in bolts with a tensile strength above 1000 MPa, so is it necessary to de-rate bolts with a lower strength than this? Can the galvanising process reduce the strength in any other way?
Thankyou
What are peoples thoughts on de-rating the tensile strength of bolts which have been galvanised?
I am designing multiple flanges which will be assembled using AS4291 / AS1110 Grade 8.8 bolts which will be galvanized. I realise that hydrogen embrittlement generally occurs in bolts with a tensile strength above 1000 MPa, so is it necessary to de-rate bolts with a lower strength than this? Can the galvanising process reduce the strength in any other way?
Thankyou