Have a query.
What is the DBTT-Ductile Brittle transition temperature for 2 1/4 Cr-1 Mo -P22/F22 chrome moly material?
Is there a formula for calculating this DBTT?
Is this DBTT valve fixed for all 2 1/4 Cr-1 Mo -P22/F22 chrome moly material?
Is there a chart available in ASTM / other standards?
DV
 
Replies continue below

Recommended for you

What AMS material standard? Or any spec
 
Last edited:
What is the DBTT-Ductile Brittle transition temperature for 2 1/4 Cr-1 Mo -P22/F22 chrome moly material?
typing that into Google gives a temperature. and some discussion, and reference papers.

Is there a chart available in ASTM / other standards?
purchase the applicable standards and review them.
 
I googled before posting here, but couldn't get.
Standard Which one? I checked ASME SA-335 but not available there.
 
This may be helpful
 

Attachments

  • API TR 938-B_2n ed. draft _Rev.13.pdf
    6.7 MB · Views: 2
And this
 

Attachments

  • timken-datos-prc3a1cticos_250225_220645.pdf
    1.7 MB · Views: 4
The DBTT for 2 1/4 Cr - 1Mo is all over the map depending on chemistry (control of C and residual elements), fine grain or coarse grain melting practice and heat treatment. It can range from around room temp to -40C.
 
And I forgot to mention product form (forged, rolled etc.) and thickness.
 