A new house is being constructed next to my client. They drove piles in the rain and crushed the pile tops. Piles were as close as 15' away. Reported damages consist of cracked concrete driveway and walkway. Both houses are on the water in a sandy location. Client's house is constructed on piles. Crawlspace slab appears to have cracked along foundation walls.
No monitoring was conducted during pile driving. Is there any literature discussing damages in order of expectations. eg glass breaks before wood before concrete. My other concern is the vibrations may cause the soil to consolidate under the driveway and crawlspace slab. Is pile driving different than blasting damages?
Thanks
No monitoring was conducted during pile driving. Is there any literature discussing damages in order of expectations. eg glass breaks before wood before concrete. My other concern is the vibrations may cause the soil to consolidate under the driveway and crawlspace slab. Is pile driving different than blasting damages?