While breaking out concrete we damaged one wire (not cut just damaged)of a 7 wire strand. The strand itself belongs with a 4 strand bonded (grouted)tendon. So in effect we have damaged 50% of the prestressing steel area of 1/28 of the tendon. The Engineering Consultant now suggests that this a huge error that is almost insurmountable. Does anyone have reference to an engineering code which would allow a reduction in prestressing area due to such site difficulties.
 
Replies continue below

Recommended for you

Try ACI 318 Section 18.18.4. This is from my 95 edition. Don't have my 2002 edition around. I do not think it has changed.
 
To add to HENRI2's reply:

ACI 318 2002 states:

18.20.4 — Total loss of prestress due to unreplaced
broken prestressing steel shall not exceed 2 percent of
total prestress.


Commentary states:

R18.20.4 — This provision applies to all prestressed concrete members. For cast-in-place post-tensioned slab systems, a member should be that portion considered as an
element in the design, such as the joist and effective slab
width in one-way joist systems, or the column strip or middle strip in two-way flat plate systems.


I have used the "2% rule" many times - sometimes a wire or two, or even a full strand may break during stressing at original construction. And during the life of the building the 'concrete coring machine' is always there to ruin your day.

I just looked at a project 2 days ago where an electrical contractor chased the underside of an existing precast/pretensioned slab panel and sawed/cut through all 7 x 1/2" strands, at MIDSPAN. Needless to say this is getting repaired with some significant $$$ being spent.

 