Ok, I hate to ask a question like this with so little detail.... but I have to as it is bugging me.
Imagine a ~4"OD flange coming off a PV. Flange is about 18" long. It has been bent out of alignment.
No PV welders are available. It needs to be put back into alignment. Solutions?