Yes we have, we can go that route but would rather reduce the chances of it occuring.
We suspect it is moisture left from cleaning after manufacturing test and then a long shipping time. We just need a less susceptible alternative to D2, some of the surfaces are aesthetically important. Would another 400 series be a better option?