JohnTM
Mechanical
- Jan 24, 2004
- 8
I need some guidance/advise/interpretation for dealing with D1.3 welder performance qualifications. Code is D1.3:2008
4.8.1.2 allows a welder to be performance qualified through WPS qualification. Let's say the test is for a non-ASTM material, like an EN10149-2 grade. Since the test would be done in accordance with D1.3, does the EN10149-2 then become "one of the steels permitted by the code" in 4.7.1.1?
Stated another way, typically I do welder qualification using a galvanized A653 Type II material from Table 1.2. Anybody who passes is qualified to weld any of the other Table 1.2 materials, per 4.7.1.1, correct? What if I have somebody do a pqr/wps on the EN10149-2 material? Per 4.8.1.2, they are then performance qualified for that combination. How do I read or interpret that they are also qualified for the table 1.2 materials? Or are they not qualified to them?
Many thanks in advance!
4.8.1.2 allows a welder to be performance qualified through WPS qualification. Let's say the test is for a non-ASTM material, like an EN10149-2 grade. Since the test would be done in accordance with D1.3, does the EN10149-2 then become "one of the steels permitted by the code" in 4.7.1.1?
Stated another way, typically I do welder qualification using a galvanized A653 Type II material from Table 1.2. Anybody who passes is qualified to weld any of the other Table 1.2 materials, per 4.7.1.1, correct? What if I have somebody do a pqr/wps on the EN10149-2 material? Per 4.8.1.2, they are then performance qualified for that combination. How do I read or interpret that they are also qualified for the table 1.2 materials? Or are they not qualified to them?
Many thanks in advance!