Hey everybody,
Welding a bunch of 1/2" fillet welds on aluminum, using ER4043.
The welders are putting in a root pass, one cover pass and then waving the cap or cover pass to complete.
They are using 3/16" tig wire and up to 1/4" tungsten.
Does anyone know the maximum weave width for AWS D1.2 using the GTAW process on a fillet weld.
The WPS says stringer or weave, I can't find anything in D1.2 2014 that limits weave width. I know the
old rule of thumb width of the cup but can we prove this in code.