What's the meaning of "D+f" on hob?
I know "WD" means whole depth. "D+f" seems the same.
 
hi asong
there is no difference between the two, its down to the manufacturers choice.
 
Thank you, lbmakem
 
According to an old gear cutter that I knew, D+f stood for Depth + fillet and was replaced by the designation WD or Whole Depth
 