Hi Everyone, I have a PQR with 6GR Position with Thickness 10 mm as per AWS D1.1 2015, my question is if I need to weld a plate with Thickness 5mm will need to have a new PQR due to thickness, which CVN is Mandatory
 
ozo1983,
Open D1.1 and have a look.
Took me about 1 minute to get the answer.
As noted on here many times previously the intent of this forum is to assist when someone cannot find something.
It is obvious you haven't even looked.
Regards,
Shane
 
Hi Shane... I don't have D1.1. Can you give me a hint?

Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?

-Dik
 
Table 4.6 (2) - Minimum thickness qualified is T or 5/8" (16 mm), whichever is less
 
Thanks...

Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?

-Dik
 