I am working on optimisation of process parameters in maraging steels using taguchi method. In this connection would anyone suggest me suitable cutting tool for turning maraging steel samples. Maraging steel i am using is 18Ni1700. Thanks in advance
 
What is suggested by Latrobe and Allvac? Look in their alloy guides.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Sandvik Coromant recommends CVD-coated tungsten carbide with elevated toughness, e.g. GC2025.
 
Thanks a lot for your valuable suggestions. I will work on it
 