carbongr
Materials
- Jul 16, 2007
- 30
I have to cut many bars of a 10mm thick carbon fibre sheet, each 1m long. The sheet is made by unidirectional fabric and high temp epoxy resin, cured in the oven.
I have tried with the band saw but the saw, (which is probably one of the best for hard metals) was ruined after just one cut.
Coolant is not an option.
Is there another way or machine i should use to do the job with high accuracy?
I have tried with the band saw but the saw, (which is probably one of the best for hard metals) was ruined after just one cut.
Coolant is not an option.
Is there another way or machine i should use to do the job with high accuracy?