Is it possible to cut axial slots to the tape wound core. 0.5mm soft magnetic iron (Fe,Ni,Si) tape, enameled and wound as ring with (or without) adhesive ( like toroid power transformer core). Both oposite flat surfaces of the core are grinded - lacquer-free , clean surfaces. OD 10", ID 8" and h - 2" , 18 slots.
I was in local EDM shop and the chief told me that it is not possible to gut with Wire EDM because the lacquer and adhesive between the winds of the iron tape. Not more explanations from this guy, the only one was - "it is not possible". May be he just does not like stupid iventors ;-)
My opinion is that "-" electrical connection comes via grinded flat surfaces of the core and all surface could be used for connection.
I dont believe that the thin film of lacquer between the winds of metal tape will break in on the process or mechanically does impede the wire.
What is your opinion?
Thanks,
Herbert
I was in local EDM shop and the chief told me that it is not possible to gut with Wire EDM because the lacquer and adhesive between the winds of the iron tape. Not more explanations from this guy, the only one was - "it is not possible". May be he just does not like stupid iventors ;-)
My opinion is that "-" electrical connection comes via grinded flat surfaces of the core and all surface could be used for connection.
I dont believe that the thin film of lacquer between the winds of metal tape will break in on the process or mechanically does impede the wire.
What is your opinion?
Thanks,
Herbert