Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Cutting Splines

Status
Not open for further replies.

rimbaldi86

Industrial
Jan 7, 2005
2
Question: I need to have a shaft manufactured for an automotive gearbox application. The shaft has a variety of diameters and bearing surfaces plus 3 splined sections. What is the best and most economical approach? Having the shaft CNC manaufactured via CAD, or manually machining the component in a lathe. What machine is used to cut splines, internal and external?

Many thanks in advance,
 
Replies continue below

Recommended for you

There are several approaches to accomplish you requirements. As you don't say whether this is a one off or a production run I would contact these people and try to locate a shop that can handle your job by Rotary Broaching.

 
One way that did it was CNC milled the splines. It was a prod run of @500 shafts a day so investment in the 4 axis MORI vmc was worth it.

The cheapest way I have heard of is spline broaching.

tell us how u finally did it.



[2thumbsup]
Work Hard and Work Smart
[2thumbsup]
 
Splines on automotive shafts are generally rolled. Very expensive dies and equipment. The next procedure is "hobbing" with something like a Barber Coleman hobber. Determining what you want to make can be very difficult because the pressure angle on an automotive part may not be a common angle. I buy hobs at Ash Gear. So far I have assumed the splines are involute. If they have straight sides, they can be made with a milling machine.