We have a customer who wants his HRS cut with nitrogen instead of O2. Does anyone have cut conditions availble for this? Also anyone know a source for conditions for odd materials? We have a Mazak 1500W. so I have the "standard" conditions they provide......Thanx sdewasme@comcast.net
 