If I need to cut ASTM F593 bolts on site, what are the requirements for treating these after the fact? Can I get away with pickling only the portion that was cut?
 
Replies continue below

Recommended for you

If these are 304 or 316 and annealed then yes, just pickle.
If these are higher strength or a ferritic alloy then you would need to bake them after pickle to assure that you avoid hydrogen embrittlement.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 