this is probably the wrong category, however i want to know if anyone has cut aluminum oxide ceramic. Is diamond the cutter?
I want to machine a pocket about .12 deep at 2" x .75" and drill 2 - 1/8" holes.
Can we use our CNC mills to do this. Any suggestions would be helpful
Thankyou