I have a Mazak Champion and having problems cutting .316 stainless. Poor cuts with dross. I'm using a 2mm nozzle. Any suggestions as to what is going on?

 
Replies continue below

Recommended for you

Make sure you have enough nitrogen pressure at the nozzle. Focal point is also important; long sharp burr means focal point is too high. Small burr means focal point too low.
 