Hi, i'm having some trouble getting cutting conditions right for an AMADA LC 3015 X1 NT. wWe normally use cold rolled stainless but just got some hot rolled in. My normal cold rolled settings will not cut. Settings i use for CR are pwr 4000, frq 1500, duty 99, feed 4200, gas pressure 9 bar (high pressure nitrogen), focus -4mm, noz gap 0.5mm, and using 2mm noz. what can i do to improve the cut quality? I'm stll getting HARD dross on the back of cut. (like a saw blade).
Thanks for any advice or help forthcoming.
Thanks for any advice or help forthcoming.