CUT OUT,REPAIR and REWELD

Status
Not open for further replies.

sunny1979

Mechanical
Joined
Oct 22, 2015
Messages
1
Location
GB
What is the detailed difference between,REPAIR,CUT OUT and REWELD?
 
Repair can mean removing the nonconforming portion of a weld, confirming that it has been removed and replacing the removed portion with weld metal and then confirming the repaired weld is sound. Cut out and Replace means just that; the complete, nonconforming weld is fully removed, the weld bevels reestablished and completely welded anew.
 