hello
i am having problems piercing and cutting .250 hrs on our amada 2415 laser.does anyone have any suggested piercing and cut conditions. all i have is the manufactured cut conditions that dont really cut that well.
 
Replies continue below

Recommended for you

What is it you're trying to cut, which version 2415 2KW 2.5 4 ??
 
im cutting A-36 PO....I get blow outs on the pierce...but when i pierce hot rolled comercial quality i do not have this problem. We have a lasmac LC 2415 cxII
 