Cut condition cutting steel with nitrogen 1

Status
Not open for further replies.

Jonathan Lessard

Mechanical
Joined
Dec 23, 2018
Messages
10
Location
CA
Hi guys I need help when I cut mild steel with nitrogen I get a small drop on corner, I really don’t know on what setting should I play with, my hole are nice and straight head cut are good. Another thing it’s only happen with 14 gauge and 11 gauge
Thank you
 
picture of my issue and my parameter
IMG_7937_znvtzp.jpg
IMG_7939_sx3oyf.jpg
IMG_7940_ltyjak.jpg
IMG_7941_ms7tgj.jpg
IMG_7942_gmjbz1.jpg
IMG_7943_mtmk00.jpg
 
hi
i am having an issue with my laser cutting machine bystronic 3015
im cutting inox 4mm and while cutting the material,
the power of laser decreases till the next part it can't be cutted,
i have lowered the speed to obtain an acceptable cutting but this doesn't resolve the problem
can anyone help?
 
sorry for the late response. most likely you have too much heat and not enough speed in the corners. crank up the modulation and play w the dwell

Chris Krug Maximum Up-time, Minimum BS
 