Anyone know how I can find more S-N curves for different materials? Solidworks only offers a handful of material curves.
 
Replies continue below

Recommended for you

a couple sources available on-line ... AR-MMPDS-01 is on the FAA web-site, or MIL-HDBK-5 .... yahoo/google "MIL-HDBK-5"
 
One more source is ASME VIII Div. 2 Appendix 5.