We have recently started using a steel vessel as a return path, instead of the cables we used to use. Current is around 1000a on a pulse fired thyristor circuit.

There have been no problem with the application, but one of our engineers has questioned the effects of passing 1000a through steel plate. Is anyone aware of any issues this could produce.
 
Well If theres not enough cross section ie: if the resistance is too high then you might get some heating. other than the standard effects of passing current through a metal object. AFAIK there are no odd or unusual rules on current carrying in steel.





Nick