I need to calculate output current of Mg anode which protects the pipeline.
I know the area of the anode. Where can I find current density for Mg (magnesium) to soil? (we know the soil resistivity)

Thanks for your help
 
Replies continue below

Recommended for you

For a CP design, the design standard will specify a current density to be achieved on the pipe surface. For example, ISO 15589-1 requires between 0.08 to 0.9 mA per square metre dependent upon pipe coating and design life. This value is then used to determine the current output requirement of the anodes.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 