Allow the concrete to cure, preferably for this case by using curing methods that prevent moisture loss and not by adding moisture to the concrete. I would cure for at least 14 days.
After curing, a temperature drawdown schedule should be followed to prevent excess cracking from thermal shrinkage and to allow moisture to be removed from the concrete more slowly to mitigate drying shrinkage and to dehumidify before reaching freezing temperatures.
ACI 302 has recommendations for a drawdown schedule (assuming you are in the US).