Hello,

I'm new to the site but have have reviewed threads within and see it is very helpful and well established source of information and advice.

I'm looking for a distributor of CuNiFe for existing projects. Also, since I'm not currently able to locate source, would also like to know possible replacement material.

I've heard that Arnokrome, Arnold Eng. is a good replacement. Are there other suppliers of CuNiFe and or other suitable replacement materials.

Thanks in advance

RHmagster
 
I used to make it for Western Electric, back in the dark ages.
Look at the Arnold material, there aren't really many options.

Do you know anyone with a small rolling mill? You could get a specialty caster if Ni alloys to cast some small ingots for you and then you could get them rolled.

= = = = = = = = = = = = = = = = = = = =
Corrosion never sleeps, but it can be managed.
 
OK, yes the technology is old.

Thanks

RHmagster
 