I am looking for a CTE for a material that is referred to as 'high Si Mo cast iron' and some refer to it as 'cast steel' though that may be a misnomer. This is a casting alloy commonly used to cast modern exhaust manifolds for gas and diesel engines. For example this is reportedly the casting alloy that GM used for the factory exhaust manifolds for several of the LS family engines. I would like to know the CTE at elevated (service) temperatures as well.

I have found a few answers here and there but they are not very consistent.

Thanks
 
Matweb is an excellent source of info such as this:

Do you know the Si and Mo percentages?
 
No I do not, I wish I did. The description I have is high Si Mo ductile iron but I see Matweb (thanks) has several alloys of that description. I'll look at their CTEs and that will at least get me in the ball park.
 