I have a CSA Z662 weld procedure that used the following materials in the PQR:
A 333 Gr 6, 406.4mm OD, 21.4mm thickness
Root: E6010
Fill and cap: E7018-1
Is this coupon automatically qualified down to -45C without conducting the impact testing? I know the A333 Gr6 and the E7018-1 have guaranteed minimum impact energies at -45C, but I am concerned about the E6010 root.
Also, I cannot find anywhere in the Z662 code where impact testing is exempt for PQR coupons if materials with guaranteed minimum impact energies are used.
A 333 Gr 6, 406.4mm OD, 21.4mm thickness
Root: E6010
Fill and cap: E7018-1
Is this coupon automatically qualified down to -45C without conducting the impact testing? I know the A333 Gr6 and the E7018-1 have guaranteed minimum impact energies at -45C, but I am concerned about the E6010 root.
Also, I cannot find anywhere in the Z662 code where impact testing is exempt for PQR coupons if materials with guaranteed minimum impact energies are used.