The RSI value of RO permeate is specified from 11 to 15.8. This value means as “severe corrosion”.
Further to the review of RSI, unexpected corrosion product and scale particle may affect to the operation and maintenance of demineralization package. pls advice me whether carbon steel is appropriate or not. if not why?