Hi all.
Most of the CS cone roof tanks that are located near sea shore regions are getting corroded rapidly. Are there any other means by which the corrosion rate can be reduced?
Replacing the CS roofs by aluminium dome roofs will not be a great idea since aluminium too will get galvanically corroded.
Suggest any other better idea.

Thanks
Vicky
 
Replies continue below

Recommended for you

Higher quality coating systems are cost-effective.
 