Continuation of this old thread: https://www.eng-tips.com/threads/crushing-of-plywood-really.371840/page-2#posts
I've been running into this issue a lot lately and having to block out the subfloor at columns. APA D510 provides a perpendicular to grain capacity of 360 psi for a 0.04" deformation. Any additional thoughts on this matter 10 years later?