Crushed Portland Cement Concrete used as Flexible Base

Status
Not open for further replies.

Drumchaser

Civil/Environmental
Aug 27, 2008
330
Does anyone have some data/comments (firsthand) on the performance of CPCC
used as flexible base? Preferably with only a chip seal as the final riding surface.

Thanks
[americanflag]











thread822-293650
 
Replies continue below

Recommended for you

Works great for that application. With chip seal you don't have to worry about reflective cracking. I would prime it though.

When hot mix asphalt is used over it, be sure you prime and tack...but expect some reflective cracking as it ages. The crushed concrete will "re-heal" with some unreacted cement, thus you will have a semi-rigid base with a flexible pavement surface...still works great though...certainly no worse with reflective cracking than soil-cement base and in my experience you have fewer cracks.
 