powerslave42
Geotechnical
I'm perfoming a modified proctor on some crushed concrete to be used as fill and all of the moistures are coming out to within about +/- 1 % of each other (about 14%), reguardless of the apparent moisture content. This seems too high to begin with, adding that to the fact that they're all coming out the same. This is the second such set of problems with 2 different samples from different locations. I have also tried both oven and microwave methods to obtain the results. Any ideas?