jam6444
Civil/Environmental
- Jan 26, 2007
- 5
I have a CMU "box" of dimensions 13'x28' with walls roughly 5' high. I'd like to fill it 90 percent with crushed concrete &then top it with some 8910, let it compact, then pour a porch slab on top. Does this sound reasonable? Clay backfill would be a no no in this instance as the walls aren't filled solid and I'm afraid the pressures would be too great. The slab will be 5"-6" thick and be reinforced to account for loads and the eventual settling of the fill below.
The crushed concrete pieces are roughly golf ball to tennis ball in size and VERY VERY irregular in shape.
The crushed concrete pieces are roughly golf ball to tennis ball in size and VERY VERY irregular in shape.