I'm trying to crush a hollow cable between two flat plates. I'm using abaqus explicit with S4R elements and a time step of 0.04s for the crushing. My problem is that the plates seem to only crush the cable elements a small way and no matter how much i increase the load (i'm using a velocity..) the displacement remains the same? Does anybody have experience of this? Should i change the contacts from self contact? Any tips or advice at all would be appreciated.
Thanks,
m.
I'm trying to crush a hollow cable between two flat plates. I'm using abaqus explicit with S4R elements and a time step of 0.04s for the crushing. My problem is that the plates seem to only crush the cable elements a small way and no matter how much i increase the load (i'm using a velocity..) the displacement remains the same? Does anybody have experience of this? Should i change the contacts from self contact? Any tips or advice at all would be appreciated.