i have problem with CSL test on test-pile with instrumented pile. but CSL test in this test pile indicated that pile has defect from depth 0-7 m (debonding)at all pair tube, and for tube pair 1-2 and 2-3 at depth 8-13.6 m (with remark 70% velocity reduction).
can anyone give technical comment regarding this CSL test, is it possible to conduct static loading test until load 250%?