I have a problem with my cross seam welder. I'm welding 0.3mm stainless steel. I am getting a good weld except for its leaving what I call a "pixie hair". At the end of th e weld it seems to pull the tiniest amount of material out and leaves this hair on the part. I have tried many things with no effect. Does anyone have any suggestions.Thanx Matt
 